Categories: Materials ScienceApplied PhysicsChemical Engineering

Preparing La0.8Sr0.2MnO3 conductive perovskite via optimal processes: High-energy ball milling and calcinations

Minghua Wang, Kee-Do Woo, Choong-Gon Lee

DOI: 10.1016/j.enconman.2010.05.013

Journal-article published March 2011 in Energy Conversion and Management volume 52 issue 3 on page 1589-1592
© Elsevier BV

Keywords: #perovskite  # resistivity  # sofc  # milling  # calcination  #sintering  Edit keywords

1 0 4.0 Posted: 02.Dec.2018

The target of the research was producing an LSM perovskite with a low resistivity, what was reached by the systematic optimization of high-energy ball milling (HEBM) (optimal time 3h), and sintering profile with a max of 1200 deg.C. Increase in calcination temperature shown to decrease resistivity. The high temperature was both increasing the reaction extent and compactness of the specimen.